uparrow-iconp0chonk

PosiTector® GLS

Gloss Meter

Portable gloss measurement for all surface finishes

  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • Weatherproof, dustproof, and water-resistant gage body—IP65-rated enclosure
  • Automatic Diagnosis and Auto Calibration performed upon power-on using the protective base plate with integrated calibration standard (tile)
  • Fast measurement speeds of 60+ readings per minute
  • 2 Powerful Scan Modes for quantifying large surfaces (Advanced models only)
  • USB, WiFi, and Bluetooth connectivity to PosiSoft PC, Mac, and Smartphone software
  • Certificate of Calibration showing traceability to NRC for both the probe and gloss standard included
Made in USA flag with black text below
Conforms to ASTM C584/D523/D4039, ISO 2813/7668, DIN 67530, JIS Z 8741, AS/NZS 1580.602.2

Features

simple icon

Simple

  • Fast measurement speed—60+ readings per minute
  • Large 2.8" impact resistant color touchscreen with redesigned keypad for quick menu navigation
  • On-gage help explains menu items at the touch of a button
  • RESET feature instantly restores factory settings
durable icon

Durable

  • All-metal probe construction for long term stability
  • Weatherproof, dustproof, and water-resistant gage body—IP65-rated enclosure
  • Ergonomic design with durable rubberized grip
  • Rugged, indoor/outdoor instrument—ideal for field or shop use
  • Shock-absorbing protective rubber holster for added impact resistance
  • Two year warranty on gage body AND probe
powerful icon

Powerful

  • Statistics mode continually displays/updates average, standard deviation, min/max, and number of readings while measuring
  • Screen Capture—save 100 screen images for record keeping and review
  • HiLo alarm audibly and visibly alerts when measurements exceed user-specified limits—can be used as Pass/Fail for quick inspection
  • Instant-on feature quickly powers up the gage if recently powered down
  • Over 20 hours of continuous operation with 3 AAA batteries
  • USB port for fast, simple connection to a PC and to supply continuous power. USB cable included
  • View pre-formatted reports and .csv data with PosiSoft USB Drive—no software installation required
  • Every stored measurement is date and time stamped
  • Includes PosiSoft Software for viewing and reporting data
  • Software Updates via web keep your gage current
accurate icon

Accurate

  • Certificate of Calibration showing traceability to NRC for both the probe and gloss standard included
  • Automatic Diagnosis and Auto Calibration upon power-on using the protective base plate with integrated calibration standard (tile)
  • Store multiple calibration standards (tiles) for quick calibration adjustment
  • Conforms to national and international standards including ISO and ASTM
versatile icon

Versatile

  • PosiTector body accepts all PosiTector probes easily converting to a coating thickness gage, dew point meter, soluble surface profile gage, soluble salt tester, hardness tester, or ultrasonic wall thickness gage
  • Selectable units for each geometry—Gloss and % Reflectance
  • Auto rotating display with Flip Lock
  • Selectable display languages

Standard Models

Includes ALL features as shown on left plus...
Includes ALL features as shown above plus...
  • Storage of 1,000 readings per probe

Advanced Models

Includes ALL features as shown on left plus...
  • Storage of 250,000 readings in up to 1,000 batches and sub-batches
  • Differential Mode automatically calculates the difference between the current reading and a stored reference value
  • 2 Powerful Scan Modes for quantifying large surfaces
    Normal – take continuous readings
    Statistics – take continuous readings and record average, standard deviation, min/max, and number of readings while scanning
  • Live graphing of measurement data
  • Touchscreen keyboard for quickly renaming batches, adding notes, and more
  • WiFi technology wirelessly synchronizes with PosiSoft.net and downloads software updates
  • Bluetooth 4.0 Technology for data transfer to a mobile device running the PosiTector App or optional portable printer. BLE API available for integration into third-party software.
  • Integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols
Includes ALL features as shown above plus...
specifications icon

Specifications

Specifications
20°
60°
85°
Measurement Area
10 x 10 mm
10 x 20 mm
4 x 45 mm
Measurement Range
0 — 2,000 GU
0 — 1,000 GU
0 — 160 GU
Repeatability
±0.2 GU (≤100 GU), ±0.2% (>100 GU)
Reproducibility
±0.5 GU (≤100 GU), ±0.5% (>100 GU)
Resolution
Gloss
% Reflectance
Haze
±0.1 GU (≤100 GU), ±1 GU (>100 GU)
0.1%
±0.1 (≤100), ±1 (>100)
Operating Conditions
0° to 45° C (32° to 113° F) - non-condensing
Probe Size
165 x 73 x 32 mm (6.5" x 2.875" x 1.25")
Probe Weight
555 g (19.6 oz.)
Gloss Range
60° value
Measure with
High Gloss
> 70 GU
20°
Semi Gloss
10 – 70 GU
60°
Low/Matte
< 10 GU
85°
PosiTector GLS kit comes complete image
ALL GAGES COME COMPLETE with protective base plate with integrated calibration standard (tile), 10 cleaning wipes, protective rubber holster, wrist strap, 3 AAA batteries, instructions, hard shell case, protective lens shield, Long Form Certificate of Calibration, USB cable, PosiSoft Software, two year warranty.
View More Features

Models

externallink-icon
View PDF Order Guide

Step 1: Choose a gage body

Step 2: Select a Model

Select up to 3 measurement angles to suit any application.
Gloss Range
60° value
Measure with
High Gloss
> 70 GU
20°
Semi Gloss
10 – 70 GU
60°
Low/Matte
< 10 GU
85°
PosiTector 200 B1 probe
GLS60-1
Application
Suitable for most gloss applications, preferred angle for semi-gloss
Geometries
60°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector 200 C1 probe
GLS2060-1
Application
Suitable for high- to semi- gloss applications — Calculates Haze (Haze Index)
Geometries
20°, 60°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector 200 D1 probe
GLS206085-1
Application
Suitable for high-, semi-, and matte- gloss applications — Calculates Haze (Haze Index)
Geometries
20°, 60°, 85°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST

Step 2: Select a Model

Select up to 3 measurement angles to suit any application.
Gloss Range
60° value
Measure with
High Gloss
> 70 GU
20°
Semi Gloss
10 – 70 GU
60°
Low/Matte
< 10 GU
85°
PosiTector 200 B1 probe
GLS60-3
Application
Suitable for most gloss applications, preferred angle for semi-gloss
Geometries
60°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector 200 C1 probe
GLS2060-3
Application
Suitable for high- to semi- gloss applications — Calculates Haze (Haze Index)
Geometries
20°, 60°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector 200 D1 probe
GLS206085-3
Application
Suitable for high-, semi-, and matte- gloss applications — Calculates Haze (Haze Index)
Geometries
20°, 60°, 85°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST

Step 2: Select a Model

Select up to 3 measurement angles to suit any application.
Gloss Range
60° value
Measure with
High Gloss
> 70 GU
20°
Semi Gloss
10 – 70 GU
60°
Low/Matte
< 10 GU
85°
PosiTector 200 B1 probe
PRBGLS60
Application
Suitable for most gloss applications, preferred angle for semi-gloss
Geometries
60°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector 200 C1 probe
PRBGLS2060
Application
Suitable for high- to semi- gloss applications — Calculates Haze (Haze Index)
Geometries
20°, 60°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector 200 D1 probe
PRBGLS206085
Application
Suitable for high-, semi-, and matte- gloss applications — Calculates Haze (Haze Index)
Geometries
20°, 60°, 85°
View PDFAdd to Instant Quote
Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST

Videos

Video Thumbnail
How to Measure Gloss with the PosiTector GLS Gloss Meter
Video Thumbnail
Saving Money and Time with PosiTector Probe Interchangeability

Software

PosiSoft Software in use

PosiSoft Desktop

Powerful desktop software for downloading, archiving, and reporting measurement data. No internet connection required.

  • Simple, intuitive user interface
  • Import readings directly from the gage via USB, WiFi, or legacy PosiSoft Desktop versions
  • Fully integrates with PosiSoft.net—backup and synchronize jobs, batches, readings, and report templates to the cloud. Click here to learn more about PosiSoft.net
Learn More

PosiTector App

An easy-to-use mobile app (iOS/ Android) that connects to your PosiTector Advanced, PosiTector Smartlink, or PosiTest AT-A. Compatible with PosiSoft.net.

Learn More

PosiSoft USB

A simple gage interface to retrieve data in a manner similar to a flash drive. No software to install or internet connection required.

Learn More

PosiSoft Custom PDF Report Generator

featured on PosiSoft Desktop, PosiSoft.net, PosiTector App
Easily create reports from your measurement data in seconds
  • Generate custom, professional PDF reports
  • Include inspection information such as on-site pictures, screen captures, notes and more to communicate important details
  • Create and save multiple custom layouts as templates – insert cover pages, add logos/images, and select font and point size
  • Select the information to include for each product type – charts, histograms, readings, time stamps and more
  • Compile multi-batch reports from one or more probes and instrument types

PosiSoft.net

PosiSoft.net is a free cloud-based application offering secure storage of PosiTector and PosiTest Inspection Instrument data. Click Here to learn more.

PosiTector Developer Resources

From wired USB to WiFi wireless technology, DeFelsko instruments offer data management solutions for even the most advanced software integrations. Accessing your stored or live streaming data is simpler and more flexible than ever before. PosiTector and PosiTest AT-A instruments have the ability to integrate with third-party software, drones, ROVs, PLCs, and robotic devices using several industry-standard communication protocols.

Learn More about Integrating Third-Party Devices and Applications

F.A.Q.

plus-icon
minus-icon

What is gloss and why is it important to measure?

Gloss is an optical property that indicates how well a surface reflects light in a specular (mirror-like) direction. It refers to how lustrous or shiny an object appears, generally affecting its aesthetic and perceived value.

Gloss measurement is useful for identifying process issues and defective parts—maximizing consistency, reducing waste, and improving quality.

For more information, see our article, "Measuring Gloss with the PosiTector GLS Gloss Meter".

plus-icon
minus-icon

What is Reflectance?

When light hits a surface, some of it is absorbed, and some is reflected. The reflected light is responsible for how the object is perceived. Reflectance as it relates to gloss measurement is the proportion of light sent and the amount of light detected.

For more information, read our article, "Measuring Gloss with the PosiTector GLS Gloss Meter" or watch our video, "How to Measure Gloss with the PosiTector GLS Gloss Meter".

plus-icon
minus-icon

What is a Gloss Unit (G.U.)?

Gloss Units are the unit of measurement typically measured and reported when measuring gloss. Gloss Units are defined by standards such as ISO 2813. Gloss meters such as the PosiTector GLS can display in both GU and percent reflectance directly on the gage.

For more information, read our article, "Measuring Gloss with the PosiTector GLS Gloss Meter" or watch our video, "How to Measure Gloss with the PosiTector GLS Gloss Meter".

plus-icon
minus-icon

What is Haze?

Haze in relation to gloss measurement is the appearance of a "milky" halo or bloom perceived in reflective surfaces.

For more information, read our article, "Measuring Gloss with the PosiTector GLS Gloss Meter" or watch our video, "How to Measure Gloss with the PosiTector GLS Gloss Meter".

plus-icon
minus-icon

Does the PosiTector GLS need to be 'calibrated' or 'adjusted' prior to use?

The innovative technology and factory calibration in the PosiTector GLS means that it arrives ready-to-measure—usually there is no need to perform a calibration adjustment. If the probe is resting in the included protective base plate and the Power-On Cal feature is enabled, the probe will automatically perform a check and calibration using the certified gloss standard (tile) incorporated in the base plate.

plus-icon
minus-icon

Does the PosiTector GLS require any formal training for use? Do you offer 'demo' models?

No. The PosiTector GLS is designed for simple operation, featuring easy-to-use menus, instruction manuals, and helpful videos. In lieu of demonstration models, we provide unlimited technical support via telephone and/or email, and a limited 30-day money back guarantee. Watch the PosiTector GLS video to see the gloss meter in action.

plus-icon
minus-icon

How often should the PosiTector GLS be recalibrated?

PosiTector GLS Gloss Meters include a Certificate of Calibration with no expiry or end date. Many organizations with a quality program and recertification programs require annual recalibrations, and this is a good starting point for most users. DeFelsko recommends that customers establish calibration intervals based upon their own experience and work environment. Based on our product knowledge, data and customer feedback, a one-year calibration interval from the date the instrument was placed in service is a good starting point.

plus-icon
minus-icon

What is the measurement range of the PosiTector GLS Gloss Meter?

PosiTector GLS Gloss Meters are available in three different models:

  • PosiTector GLS 60° — Suitable for most gloss applications (0–1000 GU)—preferred angle for semi-gloss.
  • PosiTector GLS 20° / 60° — Ideal for high- to semi-gloss surfaces (0–2000 GU)—also capable of calculating Haze Index.
  • PosiTector GLS 20° / 60° / 85° — Suitable for all gloss applications including high-, semi-, and matte-gloss—also capable of calculating Haze Index.
plus-icon
minus-icon

How many readings can the PosiTector GLS Gloss Meter store into memory?

The PosiTector GLS Standard is capable of storing up to 1,000 readings into memory. The PosiTector GLS Advanced can store up to 250,000 readings in 1,000 batches. Both Standard and Advanced models feature a USB port and include a USB cable to download, view, and print stored readings quickly and easily with PosiSoft Desktop.

plus-icon
minus-icon

How fast can the PosiTector GLS Gloss Meter measure?

By default, PosiTector GLS Gloss Meter Standard models can take 60+ readings per minute. With an Advanced PosiTector gage body, 2 powerful scan modes (Normal and Statistics) allow for even faster and more efficient measurements.

plus-icon
minus-icon

What is the HiLo Alarm Mode for the PosiTector GLS?

Available on both PosiTector GLS Standard and Advanced models, HiLo Alarm Mode audibly and visibly alerts when measurements exceed user-specified limits, and can be used as Pass/Fail for quick inspection. View the following video for an example of how HiLo Alarm Mode works.

plus-icon
minus-icon

What is the Normal Scan Mode for the PosiTector GLS?

The PosiTector GLS Advanced features a "Normal Scan Mode" for making short work of measuring gloss over large surfaces. View the video for an example of how Normal Scan Mode works.

plus-icon
minus-icon

What is the Statistics Scan Mode for the PosiTector GLS?

The PosiTector GLS Advanced features a "Statistics Scan Mode" for measuring gloss levels. Take continuous readings and record average, standard deviation, min/max, and number of readings while scanning. View the video for an example of how Statistics Scan Mode works:

plus-icon
minus-icon

Have a question that is not answered here?

Contact Technical Sales or fill out the sales form for more information. Our highly trained technical sales team is ready to answer all questions including application assistance, instrument technical support, quality and calibration, order status, sales accounting, shipping, or general information.

plus-icon
minus-icon

Still need help?

Before returning your gage or instrument for service, review the troubleshooting steps on the Troubleshooting guide, or speak with a member of our technical support team by calling +1-315-393-4450.

Accessories

PosiTector Gage BodiesPosiTector Gage Bodies

PosiTector Gage Bodies can be used with all PosiTector probes. Choose from Standard or Advanced models.

Learn MoreLearn More
PosiTector ProbesPosiTector Probes

PosiTector bodies accept all PosiTector probes easily converting from a coating thickness gage to a surface profile gage, dew point meter, soluble salt tester, hardness and ultrasonic thickness gage.

Learn MoreLearn More
Bluetooth PrinterBluetooth Printer

Battery-operated and light weight, this Bluetooth Printer prints readings and statistical summaries via Bluetooth from Advanced models.

Learn MoreLearn More
AC Power KitAC Power Kit

Use for continuous operation. This kit supplies several alternate power solutions for your battery-operated PosiTector. Operate your gage without the need for batteries.

Learn MoreLearn More
Cleaning KitCleaning Kit

10 pack of replacement cleaning wipes for the PosiTector GLS

Learn MoreLearn More
Belt ClipBelt Clip

Belt Clip for PosiTector gage bodies

Learn MoreLearn More
Protective Lens ShieldProtective Lens Shield

Pack of 5 thin plastic lens shields to protect PosiTector display from paint overspray. One lens shield included in every PosiTector purchase.

Learn MoreLearn More

Resources

Downloads

Information