Overview: Rugged, fully electronic coating thickness gauges use magnetic and eddy current principles to measure coating thickness on both ferrous and non-ferrous metals, accurately and quickly.
 
  • Ready to measure-no calibration adjustment required for most applications
  • One-Handed menu navigation
  • Bi-color indicator light-ideal in a noisy environment
  • RESET feature instantly restores gauge to factory settings

 

  • Solvent, acid, oil, water and dust resistant-meets or exceeds IP5X ingress protection
  • Wear-resistant probe tip
  • Thick, impact and scratch resistant Lexan® display suitable for harsh environments
  • Protective rubber holster with quick-release belt clip and probe storage
  • Two (2) year warranty on gage body and probe.

 

  • Certificate of Calibration showing traceability to NIST included
  • Built-in temperature compensation ensures measurement accuracy
  • Hi-RES mode increases gages displayed resolution for use on applications that require greater precision
  • Conforms to national and international standards including ISO and ASTM

 

  • Multiple calibration adjustment options including 1 point, 2 point, known thickness and average zero
  • Calibration Lock
  • SSPC PA2 feature set determines if film thickness over a large area conforms to user-specified min/max levels (memory (3) gauges only)
  • PSPC 90/10 feature determines if a coating system complies with an IMO performance standard for protective coatings (memory (3) gages only)
  • Selectable display languages
  • Flip Display for right-side-up viewing
  • Backlit display for dim or dark environments
  • Mils/Microns/mm switchable
  • Extended cables available (up to 250 ft/75 m) for remote measuring
  • All Regular Separate Probes suitable for underwater use
  • All PosiTector 6000 Gauges are available in your choice of Basic, Standard and Memory configurations
  • Menu-driven user interface with multilingual support including: English, Spanish, French, German, Portuguese, Chinese, Japanese, Norwegian, Russian, Czech and Italian - Gauge Screen Captures

 

  Coating thickness gages, gauge use magnetic and eddy current principles to measure coating thickness on both ferrous and non-ferrous metals.
 
 
 

PosiTector 6000 Memory (3) models feature
Bluetooth Wireless Technology for immediate
data transfer of readings to your PC or
compatible Bluetooth device.
 
 
 
Coating Thickness Gage measures  film thickness of coating applied to all metal substrates.