PosiTector® SST  Abrasives Test Kit

Measures the concentration of water-soluble contaminates in blast cleaning abrasives

The Abrasives Test Kit for the PosiTector SST was designed to determine the concentration of soluble salt contaminates in blast cleaning abrasives, in accordance with ASTM D4940.

Green check graphic denoting that an item is in stock
In Stock
Same-day shipping if ordered by 2PM EST
PosiTector SST with syringe

Features

simple icon

Simple

  • Quickly test abrasives for soluble salt contamination in the field or in the laboratory
  • Includes everything required to measure abrasive contamination using a PosiTector SST or other conductivity meter
  • Portable -- includes a durable, hard shell case
accurate icon

Accurate

  • Specifically designed for ASTM D4940
  • Includes certified conductivity standard (calibration solution) to verify meter accuracy. Certificate of Analysis included.

Consumables

Certified Conductivity Standard (60 ml)
To verify meter accuracy

Deionized Water (250 ml or 1L)
Purified, ion-free water

Circle Filters (100 pack)
125 mm for use with Abrasives Test Kit

Case Size: 43 x 36 x 17 mm (17" x 14" x 6.75")

Weight: 3.7 kg (8.25 lbs)

Kit Contents

  • 600 ml glass beaker
  • 100 ml glass beaker
  • 600 ml plastic beaker
  • Plastic funnel
  • 60 ml Certified Conductivity Standard
  • 1 liter deionized water (type II)
  • 100 circle filters (125 mm)
  • Stainless steel mixing rod
  • Instruction card
  • Certificate of Analysis
Image of PosiTector SST Abrasives Test Kit