PosiTest AT Adhesion
Tester Dollies

Dollies

Loading fixtures, pull stubs for testing the bond strength of coatings to metal, wood, concrete and other rigid substrates. For use with the PosiTest AT series of adhesion testers. Additional dollies available for conforming to ASTM C1583 (tensile strength of concrete overlays) and BS EN 12004 (cementitious adhesives). Multipacks offer larger quantities at a reduced cost.

Certified Coated Metal Plates & Polystyrene Blocks

20 mm Dollies

Ideal for testing the adhesion of higher bond strength coatings on metals > 3.4 MPa (500 psi)

PosiTest AT-M: 0.7 to 20 MPa / 100 to 3,000 psi
PosiTest AT-A: 0.7 to 24 MPa / 100 to 3,500 psi / 220 to 7,550 N

Name/Description
Quantity
Order Code
20 mm - 10 pack*
20 mm - 100 pack*

100

DOLLY20

10

DOLLY20APK100

Certified Coated Metal Plates & Polystyrene Blocks

50 mm Dollies

Ideal for testing the adhesion of lower bond strength coatings on wood, concrete, and plastic

PosiTest AT-M: 0.1 to 3.3 MPa / 16 to 480 psi
PosiTest AT-A: 0.1 to 3.8 MPa / 16 to 560 psi / 220 to 7,550 N

Name/Description
Quantity
Order Code
50 mm - 4 pack*
50 mm - 50 pack*

50

DOLLY50

4

DOLLY50APK50

Certified Coated Metal Plates & Polystyrene Blocks

14 mm Dollies

Ideal for testing adhesion of very high bond strength coatings on metals. Compatible with PosiTest AT 20 mm Stand-off

PosiTest AT-M: 1.4 to 40 MPa / 200 to 6,000 psi
PosiTest AT-A: 1.4 to 50 MPa / 200 to 7,000 psi / 220 to 7,500 N

Name/Description
Quantity
Order Code
14 mm - 10 pack*
14 mm - 100 pack*

100

DOLLY14

10

DOLLY14APK100

Certified Coated Metal Plates & Polystyrene Blocks

10 mm Dollies

Ideal for testing adhesion of very high bond strength coatings on metals. Compatible with PosiTest AT 20 mm Stand-off

PosiTest AT-M: 2.8 to 70 MPa / 400 to 10,000 psi
PosiTest AT-A: 2.8 to 96 MPa / 400 to 14,000 psi / 220 to 7,500 N

Name/Description
Quantity
Order Code
10 mm - 10 pack*
10 mm - 100 pack*

100

DOLLY10

10

DOLLY10APK100

Certified Coated Metal Plates & Polystyrene Blocks

50 mm C1583 Dollies

Ideal for testing the bond strength of concrete surfaces and cementitious overlays per ASTM C1583 and EN 1542

PosiTest AT-M: 0.1 to 3.3 MPa / 16 to 480 psi
PosiTest AT-A: 0.1 to 3.8 MPa / 16 to 560 psi / 220 to 7,550 N

Name/Description
Quantity
Order Code
50 mm C1583 Dolly*

DOLLY50C

2

Certified Coated Metal Plates & Polystyrene Blocks

50 x 50 mm Tile Dollies

Ideal for testing cementitious tile adhesives per EN 12004-2

PosiTest AT-M: 0.1 to 2.585 MPa / 13 to 375 psi
PosiTest AT-A: 0.1 to 3.0 MPa / 13 to 440 psi / 220 to 7,550 N

Name/Description
Quantity
Order Code
50 x 50 mm Dolly*†
50 x 50 mm Plate*

4

DOLLY50T

4

PLATE50T

†50 x 50 mm Dolly comes complete with qty. 4 plates and reusable threaded posts. Additional Plates are available separately.

‍

For use with the PosiTest AT